摘要: This document presents the results of Phase 1 of an experimental program to determine the collapse pressures of small-scale pressure hulls (ring- stiffened cylinders) with various amounts and patterns of simulated material loss due to corrosion. Six ring-stiffened aluminium cylinders have been tested as part of Phase 1: two undamaged specimens, three specimens with simulated localized corrosion, and one specimen with reinforced hull penetrations. Material loss was found to decrease the collapse pressure of each of the corroded specimens relative to similar undamaged cylinders. This loss of strength was attributed to reduced structural stiffness in the corroded regions, and was typically associated with an early onset of material yield. In two cases, yielding occurred at the corrosion well before the ultimate collapse load, and would thus further decrease the allowable working load. The results of the entire experimental program, which will include upwards of 40 cylinders, will be used to develop guidelines for corrosion tolerance, and to validate analytical and numerical methods. / NOTE: Technical memorandum. / Supplementary Notes: The original document contains color images. / Availability Note: Order this product from NTIS by: phone at 1-800-553-NTIS (U.S. customers); (703)605-6000 (other countries); fax at (703)605-6900; and email at orders@ntis.gov. NTIS is located at 5285 Port Royal Road, Springfield, VA, 22161, USA.
总页数: u0809;112p
报告类型: 科技报告
检索历史
应用推荐